Lithium Nickel Aluminum Cobalt Oxide (NCA) - 5 micron particle size

BNCAn-25
  • Lithium Nickel Aluminum Cobalt Oxide (NCA) - 5 micron particle size
  • Lithium Nickel Aluminum Cobalt Oxide (NCA) - 5 micron particle size
  • Lithium Nickel Aluminum Cobalt Oxide (NCA) - 5 micron particle size
  • Lithium Nickel Aluminum Cobalt Oxide (NCA) - 5 micron particle size

Please

Register and login to see price


Lithium Nickel Cobalt Aluminum Oxide material - battery grade - produced in large volume production line. This Lithium Nickel Cobalt Aluminum Oxide material is also used in commercial battery production. Lithium Nickel Cobalt Aluminum Oxide (NCA) material has optimum particle size - used in batteries with high energy or high power applications. Lithium Nickel Cobalt Aluminum Oxide (NCM) has lower iron impurity for higher safety. Average particle size is 12-16 micron.

 Specifications

  • Form: Powder
  • Chemical formula: Li(Ni0.80Co0.15Al0.05)O2
  • Nominal Voltage: 3.6V vs Li/Li+
  • Tap Density: NA
  • Average Particle Size D50: 5µm
  • Nominal Capacity at 0.05C: 185 mA/g
  • Iron Content < 20 ppm
  • Color: Black
  • Shelf life: 3 months
  • Storage: Dry atmosphere
  • Surface area: 0.2 to 0.5 m2/g (BET)

 